Abstract

In the present investigation, PLA porous scaffolds was fabricated using NaCl as porogen in three different solvents i.e. 1,1,1,3,3,3-hexafluoro-2-propanol (HFIP), dichloromethane (DCM) and chloroform (CF) respectively, by solvent casting particulate leaching method. The morphology, structure and thermal behaviour of the PLA scaffolds for porosity measurement were evaluated using scanning electron microscopy (SEM), Fourier transform infrared spectroscopy (FTIR); thermo gravimetric analysis (TGA) and differential scanning calorimetry (DSC). The developed porous scaffolds were further characterized for porosity measurement, solvent uptake property and water absorption capacity at different temperatures. PLA/ CF scaffold depicted higher porosity factor (93%) along with enhanced water uptake capacity (220%) as against PLA/ HFIP scaffold (75%). However PLA/ DCM scaffolds illustrated more thermal stability as compared with PLA/ HFIP and PLA/ CF scaffolds.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.