Abstract
The aim of this study was to evaluate and compare microhybride composite treated by bur and different power of Erbium, Chromium doped Yttrium Scandium Gallium Garnet (Er,Cr:YSGG) laser by Scanning Electron Microscope (SEM). 21 microhybride composite blocks (DiaFil TM, DiaDent, Korea) with 2 × 4 × 4 mm dimensions were made. The bonding surface of these blocks were polished, The samples were put into 6 groups for laser irradiation as follows: Group 1 (power: 1W, Energy: 50 mJ); Group 2(power: 2 W, Energy: 100mJ); Group 3 (power: 3W, Energy: 150mJ); Group 4 (power: 4W, Energy: 200mJ); Group 5 (power: 5W, Energy: 250mJ) and Group 6(power:6 W, Energy:300mJ). One group prepared by bur- treated. All samples were prepared by repetition rate of 20 Hz. Then, the samples were prepared for SEM examination. Some irregularities were seen in Er,Cr:YSGG laser samples in comparison to Bur group that produced favorable surface for adhesion of repair composite. Among different lasers, Er;Cr:YSGG laser can be chosen as a suitable technique for surface treatment of unsatisfactory composites.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.