Abstract

The increasing demand for excellent steel properties has led to the creation of new steel grades such as high manganese TWIP and TRIP steels which are scientifically examined in Germany within the international research framework of the SFB 761 “Steel-ab initio.” The production of these high-technology products, utilizing mainly the ingot-casting method, leads to new challenges in the prevention of cast defects. At RWTH Aachen University, a systematic investigation of the solidification process as it relates to shrinkage cavity, macrosegregation, cleanliness, and surface imperfections in as-cast ingots is being conducted. A particular attention was devoted to the effects of such casting parameters as superheat, pouring rate, hot top, and stirring conditions on the solidification and cleanliness of low carbon alloyed and high manganese alloyed steels. The experimental results show that rising manganese content leads to a higher amount and larger size of inclusions while rising carbon content enhances the inclusion generation in the same way. It was found that a bottom teeming system combined with an inert gas atmosphere produces the best quality and that if casting is performed with a runner-system, it is important to use a SiO2-free refractory to avoid oxidizing the Mn content of the melt to MnO inclusions by redox-reactions.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.