Abstract

This paper reports the material properties of Cr3+ (1.0 mol%)-doped ZnGa2O4 nanopowders prepared by citric acid-assisted sol–gel method with metal cations (Zn + Ga) to citric (M:CA) molar ratios of (1:0.5, 1:1, 1:3 and 1:4). The X-ray diffraction (XRD) results show that the synthesized nanoparticles are cubic structured and concentration of citric acid did not affect the structure. The scanning electron microscope (SEM) shows that the increase of the M:CA molar ratio favors the formation of smaller nano particle of ZnGa2O4:Cr3+. The photoluminescence (PL) is found to be maximum for sample with M:CA ratio of 1:1. Further increase in citric acid leads to significant decrease in the PL intensity. Energy-dispersive X-ray spectroscopy (EDS) measurement confirms the presence of the Zn, Ga, O and Cr ions. Ultraviolet–visible (UV–Vis) spectrophotometer measurement shows an increase in reflectance in visible region and the energy band gap was found to decrease with an increase in citric acid molar ratio. The emission spectra, particle size and photoluminescence lifetimes are comparable with reports on bioimaging applications.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.