Abstract

ABSTRACTThe effect of CaO on the reduction behaviour of iron ore–coal composite pellets has been studied in a laboratory scale multi-layer bed rotary hearth furnace at 1250°C for 20 min. Reduced pellets have been characterised through weight loss, porosity measurement, phase analysis by XRD, and morphology study by SEM. The addition of CaO to the composite pellets showed different effects at different carbon levels. For higher carbon-containing pellets (C/Fe2O3 molar ratio at the upper stoichiometric level of 3), the addition of CaO increased the extent of reduction for all three layers significantly up to a certain limit (4 wt-%); and thereafter the degree of reduction is decreased with a further increase in CaO percentage in the pellets. For low carbon-containing pellets (C/Fe2O3 molar ratio of 1.66), the addition of CaO to the pellets did not show any beneficial effect.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.