Abstract

The passivation behavior of Fe–Al alloys (3.4, 10.4, 18.7, 19.4, 29.5, and 41.7 at % Al) and Fe–Al alloys (19.5 and 29.0 at % Al) with 5.1 at % Cr addition in 0.1 N H2SO4 is reported in this paper. The behavior has been evaluated by potentiodynamic polarization measurements. The results show the Fe–Al alloys, which the Al content of alloy exceeds 19 at %, have wide passivation regions with low passivation current. However, when the Al content of Fe–Al alloys exceeds this range, the increment of Al content has slight influence on passivation behavior compared with ternary Cr addition.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.