Effect of acidic pretreatment of arsenic-bearing gold concentrate, a promising gold source, on its chemical composition and efficiency of its bacterial oxidation (BO) was studied. The titer of sulfobacilli during BO of the concentrate after high-temperature acidic treatment was 9.0 x 10(7) cells/ml, the degree of arsenic sulfide oxidation being 71.1%, and in the control, 6.5 x 10(7) cells/ml with the oxidation degree as low as 48.7%. Deeper oxidation of the main gold-containing mineral, arsenic sulfide, would allow more efficient gold recovery from the concentrate.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.