Galvanic corrosion performance of 5383 Al alloy coupled with 907 steel and aluminum bronze respectively in the early stage was studied by galvanic current test and scanning electron microscopy(SEM). The results showed that the 5383 Al alloy acted as anodes for the two galvanic couples, while 907 steel and aluminum bronze were cathode. The corrosion morphology of 5383 Al alloy could be metastable pitting, irregular stable pitting and filiform- like corrosion. The galvanic current density Igof two couples varied similarly with immersion time, they decreased at the beginning and then became stable. The galvanic current density decreased with the increase of distance from the couple joint, and it became uniform in the far end. Compared with the couple 5383 Al alloy/aluminum bronze, the galvanic corrosion for couple 5383 Al alloy/907 steel was less severe,but it was more concentrated with in an area of 2 mm nearby the joint line.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.