Macroscopic and microscopic drying patterns were observed on a cover glass, a watch glass, and a Petri glass dish during the course of dryness of aqueous suspensions of similar sized aggregates of diamonds (CD1), which formed from the deionization of the pre-particles of diamond 4 nm in diameter. Two kinds of macroscopic patterns, i.e., outer and inner broad rings, and spoke lines were formed. Cooperative drying processes of the convection, sedimentation, and solidification were clarified. Microscopic drying patterns showing the formation of very large dendritic aggregates from the CD1 particles were observed only when the excess amount of sodium chloride higher than 2 mM coexisted in the initial suspensions before dryness and further initial CD1 concentration is lower than 0.17 wt%.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.