Double torsion tests were performed to study subcritical crack growth of a 3Y-TZP ceramic. A significant variation of stress intensity factor K 1 with crack length was observed. In order to take into account this variation a correction factor is introduced into the well-known analytical expression of stress intensity factor in mode I. This has enabled us to obtain accurate crack growth parameters i.e. an accurate measurement of (i) the three propagation stages of the subcritical crack growth and (ii) a threshold value equal to K IO = 3.5 MPa√m. Analytical expression of K 1 based on a compliance analysis was shown to be unsatisfactory for slow crack growth analysis because of the influence of the unbroken ligament on the compressive side arising from the curved crack front.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.