Abstract
We present low field dc magnetization (M) measurements on the amorphous alloys (Fe1−xMnx)75P16B6Al3 for x≲0.35. Analysis shows that the spontaneous M goes to zero as T→TC− and Tf+ while the dc susceptibility diverges with T→TC+ and Tf−. It is demonstrated that the ferromagnet–spin glass transition line is significantly different from that obtained by scaling analyses of high field M data.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.