Abstract

The phase separation processes occurring in poly(l-lactide) (PLLA)−chloroform−methanol mixtures and poly(dl-lactide) (PDLLA)−chloroform−methanol mixtures have been studied using differential scanning calorimetry, cloud point measurements, and optical microscopy. It is demonstrated that liquid−liquid demixing occurs in ternary solutions of PDLLA at sufficiently high methanol concentrations. For PLLA-containing solutions, both liquid−liquid demixing processes and solid−liquid demixing processes occur. The most important parameters for the phase separation process are the applied cooling rate and the polymer concentration. Nonequilibrium phase separation processes play an important role in the phase separation of ternary PLLA solutions. Due to the high activation energy needed for crystallization, liquid−liquid demixing will usually precede solid−liquid demixing even if solid−liquid demixing is favored thermodynamically. Only at low cooling rates and high polymer concentration does solid−liquid demixing take...

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.