Abstract

The brass foil with a protective layer formed on one side was deflected during original corrosion in 1 mol⧹L NH 4OH+5 g⧹LCuCl 2 solution. This was due to corrosion-induced tensile stress developed in the dezincification layer of the sample. The additive tensile stress grew gradually, and reached a steady value of about 24.4 MPa, i.e., 20% of the yield stress of brass.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.