Abstract

The conditions of ceramic nanopowder compaction essentially influence the quality and properties of sintered ceramics. Methods for determination of important parameters of nanopowder dry compaction with regard to powder body elastic properties are presented for the following parameters: powder body elastic modulus and sound velocity; Poisson ratio; coefficients of internal friction, wall friction, lateral pressure; elastic aftereffect in height and diameter; density uniformity; green compact quality parameter. The influence of ultrasound action of different power on these characteristics is shown. The experimental dependences of the compaction parameters of ZrO/sub 2/-Y/sub 2/O/sub 3/ nanopowder on compaction pressure, ultrasound power are analysed. Conclusions about the effective range of nanopowder ultrasonic compaction are obtained.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.