Abstract

Several 35CrMo4 and 38MnV7 steels with different additions of Ti and V were manufactured by electroslag remelting. The influence of the alloying and microalloying elements on phase transformation at different cooling rates was studied and the continuous cooling transformation diagrams were plotted. In order to optimize the heat treatment and improve the mechanical properties, the range of cooling rates leading to a fully bainitic microstructure (without ferrite, pearlite and especially without martensite) was determined. Bainite and martensite transformation start temperatures (Bs, Ms) were also established and compared with the values predicted by empirical equations. The important role of precipitates (especially V carbonitride particles) on final microstructure and mechanical properties was assessed.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.