Abstract

Laser surface melting (LSM) on sensitized austenitic stainless steel of cold‐work 25 per cent was carried out by using a continuous wave CO2 laser of power 5kW and traverse speed 20mm/sec of the beam. The stainless steel was sensitized at 898K for 10, 20 and 50hr durations. ASTM A262 Practice A test was used to examine the microstructures of the specimens before and after LSM while single loop electrochemical potentiokinetic reactivation (SL‐EPR) technique was used to quantify the degree of sensitization (DOS). A trend is noted between the cold‐work of stainless steel and the degree of desensitization by LSM.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.