ABSTRACT The composition of CaO-SiO2-MgO-Al2O3-CaF2 slag was designed by thermodynamic calculation of [Al]-[O] equilibrium of FeNi-based expansion alloy. On this basis, the deoxidation and inclusion evolution in the process of slagging and smelting FeNi-based expansion alloy in the medium frequency induction furnace were investigated. The results show that the oxygen content in the alloy melt is mainly controlled by the [Fe]-[O] equilibrium, and the change trend of the equilibrium oxygen content calculated by [Fe]-[O] equilibrium is consistent with the actual oxygen content. The total oxygen content of the final ingot is 45 ppm. After Al deoxidation in the melting process, the inclusions in the alloy are transformed into composite oxide inclusions rich in Al2O3 and MgO. After final deoxidation with Si-Ca alloy, the contents of Al2O3 and MgO in the inclusions decreased significantly, while the CaO content increased. And there are mainly CaO-SiO2-MgO-Al2O3 composite oxide inclusions in the ingot.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.