Abstract

We investigated the densification of undoped, nanocrystalline yttria (Y2O3) powder by spark plasma sintering (SPS) at sintering temperatures between 650°C and 1050°C at a heating rate of 10°C/min and an applied stress of 83 MPa. In spite of the low sinterability of the undoped Y2O3, a remarkable densification of the powder started at about 600°C, and a theoretical density of more than 97% was achieved at a sintering temperature of 850°C with a grain size of about 500 nm. The low temperature SPS is effective for fabricating dense Y2O3 polycrystals.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.