Abstract

Dense and translucent BaZrxCe0.8−xY0.2O3−δ (x=0.5, 0.6, 0.7) proton conductors were firstly and successfully prepared by Spark Plasma Sintering (SPS) at a temperature of 1350°C without sintering aids’ addition. XRD, SEM and EDS were applied to determine the phase purity, morphology and element composition of prepared pellets, respectively. Moreover, the sintering behaviors of these proton conductors were monitored and analyzed through the on-line sintering curves. The obtained results indicate that a lowered sintering temperature (<1400°C) and a fast cooling rate (⩾200°C/min) represent two key parameters to prepare dense Ce-containing BaZrO3–BaCeO3 based proton conductors.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.