Abstract
The pattern of dendritic growth and distortion of dendritic network in the platform have been investigated by one mold casting with different platform length during directional solidification. As the platform length elongates, the symmetry of dendritic growth along left and right edges gradually worsens in platform base. While the platform length reaches 14 mm, the distortion of dendritic network is first observed in outward platform. It is found that the distortion of dendritic network along platform inside is more serious than that along platform edges. Both [001] deviation and accumulated misorientation along platform inside, up to 9° and 16.3°, respectively, are far greater than those along left–outward–right edges. The deformation of dendritic network in a platform may be caused by the asymmetry of the solidification front at the mush zone.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.