Abstract

Thermal degradation was performed at 175, 200, and 250 °C from 100 to 2000 h on flame‐retardant ethylene propylene rubber (FR‐EPR) with the same compositions as those used in the insulation of a safety‐related cable in nuclear power plants. For these samples, indenter modulus (IM), elongation at break, tensile strength, and complex permittivity were measured to clarify mechanical and dielectric properties. Fourier transform infrared absorption and differential scanning calorimetric spectra were also measured to determine structural changes. As a result, it was found that FR‐EPR becomes hard by oxidation and crosslinking, and that it becomes brittle as the degradation becomes more severe. In addition, such changes in mechanical properties by the aging occur much earlier than the changes in dielectric properties. Regarding this, IM is a good indicator to examine the degradation degree of FR‐EPR. © 2020 Institute of Electrical Engineers of Japan. Published by John Wiley & Sons, Inc.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.