Abstract

The objective of this study was to investigate the degradability of linear low‐density polyethylene (LLDPE)/(soya powder) blends. The blends were compatibilized by epoxidized natural rubber with 50 mol% of epoxidation. They were exposed to a natural compost medium located in northern Malaysia. The degradability was evaluated by using tensile tests, a morphological study, carbonyl indices, crystallinity measurements, weight loss, and molecular‐weight changes. The tensile strength and elongation at break of the compatibilized blends decreased during one year of exposure. The colonization of fungus and the formation of pores were observed in micrographs. The carbonyl indices, crystallinity, and weight loss increased during exposure, thereby indicating the degradation of the blends. The reduction in molecular weight revealed the degradation of the LLDPE upon composting. Surprisingly, after composting, the compatibilized blends showed more degradation than the uncompatibilized ones. J. VINYL ADDIT. TECHNOL., 20:42–48, 2014. © 2014 Society of Plastics Engineers

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.