Cooling time in the temperature range 800 - 500°C has a great effect on the structures that arrise in the heat affected zone of welds steel. Data on optimal cooling time t8/5 for the certain steels can be found in the literature. The period of the cooling time t8/5, during the welding of the particular joints, in addition to the thickness and physical properties of welded steel, depends on shape of the weld, the welding process and welding parameters as well. In this work, the procedure for the selection of welding parameters for a butt joint welded to the microalloyed steel P 460 NL1 is presented. The microstructure in the heat affected zone and the results of measurement of their hardness are showed and analysed. It is concluded that the welding parameters selected with the help of cooling time t8/5 provide the satisfactory structure and hardness of welds.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.