Glycerol dry reforming (GDR) turns glycerol and CO2 into valuable syngas. The present work aims to decipher the imperative role of Ru metal in enhancing the performance of Ni/Nd2O3.Gd2O3 in GDR. The unpromoted 15%Ni/Nd2O3.Gd2O3 and promoted 3%Ru-Ni/Nd2O3.Gd2O3 catalysts are synthesized via the ultrasonic-assisted impregnation method while XRD, FESEM-EDX, H2-TPR and CO2-TPD analyses are used to characterize the catalysts. In this study, the influence of reaction variables such as temperature and the CO2 to glycerol ratio (CGR) was investigated. In accordance with XRD and FESEM-EDX analyses, the promoted catalyst exhibited a more refined morphology and more uniform Ni dispersion than the unpromoted catalyst. From the reaction study, the promoted 3%Ru-15%Ni/Nd2O3.Gd2O3 gives higher glycerol conversion (91%), H2 yield (65%) and CO yield (80%) at a reaction temperature of 800 °C and CGR of 1. This is due to the higher number of available active sites as well as the excellent diffusion of Ni metal across the surface of the catalyst. However, as Ni metal is susceptible to carbon formation and is easily sintered, the production of carbon is unavoidable for the catalysts. The XRD and TPO analyses shown that the addition of Ru reduces the amount of carbon that accumulates on the site of the catalyst, which in turn reduces the rate of deactivation.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.