Abstract

The relative rates of deamidation, acylation and proteolysis (i.e. amide bond cleavage) were determined for a model peptide (VYPNGA) in poly ( dl-lactide-co-glycolide) films. Films were stored at 70 °C and either 95%, 75%, 60%, 45%, 28%, or ∼0% relative humidity and at 37 °C and 95% relative humidity. Peptide degradation products were identified by ESI+ MS/MS and quantitated by LC/MS/MS. Extensive overlap of degradation mechanisms occurred, producing a complex mixture of products. Acylation was the dominant peptide degradation reaction (10–20% of total peptide) at early stages of PLGA hydrolysis and at intermediate relative humidity (60–45% RH). Deamidation and proteolysis were dominant (25–50% and 20–40% of total peptide, respectively) at later stages and at high relative humidity (95–75% RH). Understanding the relative rates of each peptide degradation reaction will allow for improved design of PLGA formulations that preserve the stability of peptide and protein drugs.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.