Abstract

Laser scanning confocal microscopy (LSCM) and Electron back-scattered diffraction (EBSD) were applied to the study of surface morphology variation of as-cast Mg–3.0Nd–0.2Zn–Zr (NZ30K) (wt.%) alloy under tension-compression fatigue test at room temperature. Two kinds of typical damage morphologies were observed in fatigued NZ30K alloy: One was parallel lines on basal planes led by the cumulation of basal slips, called persistent slip markings (PSMs), and the other was lens shaped, thicker and in less density, led by the formation of twinning. The surface fatigue damage morphology evolution was analyzed in a statistical way. The influences of stress amplitude and grain orientation on fatigue deformation mechanisms were discussed and the non-uniform deformation among grains and the PSMs, within twinning were described quantitatively.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.