Abstract
AbstractThe crystallization of poly(vinylidene fluoride) (PVDF)/poly(3‐hydroxybutyrate) (PHB) blends was studied with differential scanning calorimetry, from which the phase diagram was derived. Strong miscibility was underlined by the large negative Flory–Huggins interaction parameter (−0.25). The crystallization of the blend components differed remarkably. Whereas PVDF always crystallized in the surroundings of a homogeneous melt, PHB crystallized in a volume that was confined by the already existing PVDF spherulites, partly in their surroundings and partly inside. Under isothermal conditions, PVDF usually crystallized regularly in three dimensions with predominant quench‐induced athermal nucleation. The Avrami exponent for PVDF dendritic spherulitic growth was, however, distinctly smaller than that for compact growth, and this revealed the two‐dimensional lamellar growth inside. This deviation from ideal Avrami behavior was caused by the development of compositional inhomogeneities as PVDF crystallization proceeded, and this decelerated the kinetics. PHB crystallized three‐dimensionally with mixed thermal and athermal nucleation outside the PVDF spherulites. Inside the PVDF spherulites, PHB crystallization proceeded in a fibrillar fashion with thermal nucleation; the growth front followed the amorphous paths inside the dendritic PVDF spherulites. The crystallization was faster than that in the melt of uncrystallized PVDF. Solid PVDF acts possibly heterogeneously nucleating, accelerating PHB crystallization. © 2004 Wiley Periodicals, Inc. J Polym Sci Part B: Polym Phys 43: 287–295, 2005
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
More From: Journal of Polymer Science Part B: Polymer Physics
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.