Eu2+, Dy3+co-doped strontium aluminate (SrAl2O4) phosphor with high brightness and long afterglow were prepared by nano pseudo-boehmite particulate sol method. The precursor was prepared by peptizing AlOOH powders with HNO3 as peptize agent. The influence of preparation parameters on crystal structure and luminescent properties of the phosphor have been studied systematically. Monoclinic SrAl2O4host with single-phase can be obtained by controlling sintering temperature at 1200°C, 4Wt%B2O3 and RSr/Al=0.34. The sample exhibits an intensive emission peak at 515 nm and the luminescent intensity decay with I=277.78t-1.079 .

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.