Cross-sectional sample preparation is one of the most important failure analysis (FA) techniques in the semiconductor industry. It was commonly used for film stack critical dimension measurement, defect identification, electrical fault isolation and etc. However, cross-sectional sample preparation to a specific target location on a sub-micron device is very challenging and time-consuming. This is because of mechanical polishing easily caused metal smear, delamination, film peel-off, micro-cracked and etc. This paper focused on cross-sectional nanoprobing (XNP) sample preparation improvement in quality and quantity. A laser blast to deprocess or create a groove at near to target location before conventional mechanical polishing and focus ion beam (FIB) fine milling. The proposed technique not only reduces the sample preparation time to the sub-micron target location but also prevent mechanical damages that caused by mechanical polishing technique.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.