Cr-doped TiO2 thin films with different band gaps were prepared. Higher Cr doping was beneficial to the formation of the rutile-TiO2 phase over the anatase-TiO2 phase. A 4.8% Cr-doped thin film indicated a band gap of 2.95eV, which was lower than the band gap of the rutile-TiO2. Cr doping was accompanied by the formation of not only the rutile-TiO2 phase but also the Cr2O3 phase, lead to the degradation of the hydrophilicity. The TiO2 thin films with the mixed phase were not desirable to improve the hydrophilicity.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.