Abstract
ABSTRACT Maraging steel 300 processed by laser powder bed fusion (PBF-LB/M) is widely used for manufacturing inserts and moulds with conformal cooling channels. For such applications, high fracture toughness and strength are required to withstand thermal fatigue and any defect like pores, lack of fusion and cracks should be avoided so that the durability of the mould is not reduced. Maraging steel is prone to be cracked due to thermal gradients which arise during PBF-LB/M. Moreover, it was recently observed that slight variations in composition led to the crack’s presence, which implied lower mechanical properties. In this study, two powder batches, from the same powder producer, were employed with the same processing parameters. The effect of small changes in minor elements composition of the powder batch on cracking was studied and the preheating temperature was varied to significantly reduce the crack density. The presence of cracks significantly reduced the ductility of the parts.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.