AbstractThe mechanical properties and cracking behaviours of rock‐like materials containing three preexisting flaws after high‐temperature treatments are studied. The temperature variations of 25°C, 70°C and 140°C are chosen to explore the influence of temperature, and the ligament angle variations of 75°, 90° and 105° are chosen to explore the effect of preexisting flaws. The crack initiation and coalescence modes and specimen failure after high‐temperature treatments are recorded by a high‐speed dynamic analysis system. Seven modes of crack initiation and ten types of crack coalescence are recorded in the rock‐like specimens. With an increase in temperature and ligament angle, the mechanical properties such as peak strength, peak strain and crack initiation stress change regularly. Furthermore, the experimental results demonstrate that the temperature has a significant impact on the complete stress–strain curves and cracking behaviours of flawed rock‐like materials.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
More From: Fatigue & Fracture of Engineering Materials & Structures
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.