Abstract

The development of cracks and changes in appearance have been investigated on radial and tangential sections of pine (Pinus sylvestris L.) and spruce (Picea abies Karst.) after exposure outdoors for 61 months. The degradation of the sections has also been studied at the micro-level. The annual ring orientation was the most important factor affecting crack development on weathering. After 61 months of outdoor exposure, the tangential sections of spruce had 1.7–2.2 times greater mean total crack length per area unit than the corresponding radial sections. In pine, the total crack length per area unit on the tangential sections was 2.2–2.6 times greater than that on the radial sections. Tangential and radial sections show the same colour change as a result of weathering. Tangential sections have more and deeper cracks than radial surfaces. The cracks on the tangential sections occur frequently in both earlywood and latewood. On radial sections, cracks occur primarily at the annual ring borders, but to a certain extent also in the earlywood. Decomposition of the cell wall takes place in both radial and tangential cell walls, and cracks tend to follow the fibril orientation in the S2-layer of the cell wall. The radial cell wall of the earlywood has a large number of pits which are degraded at an early stage.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.