Abstract

Measurements of wall loss of syngas cooler tubes (T-11) were done in an IGCC pilot plant which was operated 4700 hours for 6.25 years. The corrosion rate is pseudo-linear and the total loss is 3.2 mm max. The scale formed consists of the layers of iron sulfide and oxide. The corrosion loss is too large for high temperature corrosion only at tube skin temperature of 230–250°C. The syngas cooler was opened to air for the shutdown time of about 59000 hours. Therefore, it is concluded that the downtime corrosion strongly contributed to the loss of tube wall in this test plant.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.