The deterioration process of a plasma electrolytic oxidation (PEO) coating containing zirconium oxides on AM30 magnesium alloy in 3.5 wt.% NaCl solution have been investigated. The coating consists of an outer porous layer and an inner dense layer. The content of MgF 2 is high in the pores and an MgO-rich layer is evident in the inner layer. The corrosion resistance of the outer layer gradually decreases in the initial immersion stage (96 h) due to the decomposition of MgO, and the deterioration of the inner layer is delayed by the blocking effect of the outer layer.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.