Abstract

The influence of substrate effects on the accurate measurement of mechanical properties of thin films remains to be clarified. Therefore, in this study, (AlCrNbSiTi)N thin films were deposited on four substrates—Si, SiO2, sapphire (Al2O3), and Ni—with varying thicknesses. Nanoindentation testing was conducted to measure the mechanical properties, revealing variations in the modulus of the thin film depending on the substrate and film thickness. To address these variations, we introduced the concept of two springs connected in series, following Hooke's law, to determine the elastic deformations of the thin film and its underlying substrate. By applying linear regression to four datasets corresponding to equivalent film thicknesses but different substrates, substrate-induced measurement errors were effectively mitigated, and the true modulus of the thin film was determined. Furthermore, we introduced a k value to represent the ratio of the actual force on the substrate to the force exerted by the indenter. Our findings indicate that even when the indenter contact depth is less than 1% of the film thickness, the substrate is still subjected to 7.6% of the applied force. This underscores the non-negligible nature of substrate elastic deformation during the measurement process and importance of correcting for substrate-induced variations in thin-film moduli. The findings can contribute to advancing the understanding of mechanical properties in ceramics and related materials.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.