ABSTRACTPolar functionality attached onto natural rubber has a significant impact on the reinforcing efficiency of silica. Parallel studies involving various levels of epoxidation on natural rubber (ENR) in the absence of bis-(triethoxysilylpropyl) tetrasulfide (TESPT) coupling agent, as well as a combination of ENRs with different loadings of TESPT, provide a better understanding of the various factors that influence the properties of silica-filled ENR compounds. Based on the overall properties, the best possible combination to optimize processability, to reduce filler–filler interaction, and improve vulcanization rate as well as vulcanizate properties, is to use ENR with an epoxide content in the range of 20–30 mol%, together with a small portion of TESPT, that is, 2–4 wt% relative to the silica content. This leads to a reduction of approximately 60–80% of TESPT when compared with the conventional NR compounds, where the optimal loading of TESPT was 9.0 wt% relative to the silica content.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.