Abstract

HfO2 thin films have been deposited onto p-Si(100) substrates by atomic layer deposition (ALD) using Cp2Hf(CH3)2 (Cp = cyclopentadienyl) and water as precursors at 300–500 °C. Processing parameters were optimised and the ALD type growth mode corroborated at 350 °C where a deposition rate of 0.42 A cycle−1 was obtained. The crystallinity, morphology and chemical composition of the deposited films were characterised. Films deposited at 300–450 °C were polycrystalline with monoclinic (−111) as the preferred orientation. Impurity levels of the stoichiometric HfO2 films deposited at 350 and 400 °C were very low, or below 0.4 and 0.25 atom% for carbon and hydrogen, respectively. In addition, ultrathin HfO2 films showed good dielectric properties such as low hysteresis and nearly ideal flatband voltage.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.