Abstract

Simultaneous shear coupling and grain rotation were observed experimentally during grain boundary migration in high-purity Al bicrystals subjected to an external mechanical stress at elevated temperatures. This behavior is interpreted in terms of the structure of the investigated planar 18.2° 〈1 0 0〉 non-tilt grain boundary with a 20° twist component. For characterization of the grain rotation after annealing under stress the bicrystal surface topography across the boundary was measured by atomic force microscopy. The temperature dependence of the boundary migration rate was measured and the migration activation energy determined.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.