Hydroxyapatite (HA) was incorporated as filler into polycaprolactone (PCL) matrix to improve the bioactivity as well as the compressive properties of the polymer composites that can be typically used in tissue engineering scaffolds. The compressive properties of five PCL/HA composites of different compositions were investigated in conjunction with the study of their rate of degradation. As PCL has a slow degradation rate, the experiment was conducted in a concentrated 5M sodium hydroxide medium to accelerate the degradation process. The compressive strength and modulus of all PCL/HA compositions were observed to decrease as the degradation experiment progressed, with samples having high HA content degraded most significantly as compared with samples with lower HA content. Pure PCL samples, however, were found to retain their mechanical properties comparatively well in the same degradation experiments. Although the addition of HA as filler into the PCL matrix was shown to have improved mechanical properties and bioactivity initially, these results do raise concerns of material properties being compromise during hydrolytic degradation.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.