Abstract

This paper examines the fundamental mechanical properties of masonry elements incorporating fired-clay bricks and hydraulic lime mortars under ambient-dry and wet conditions, corresponding to 48 h submersion in water. In addition to complementary material characterisation assessments, two types of specimens are tested: cylindrical cores in compression, and wall elements in compression. Overall, a detailed account of more than 50 tests is given. Apart from conventional measurements, the use of digital image correlation techniques enables a detailed assessment of the influence of moisture on the constitutive response, confinement effects and mechanical properties of masonry components. The uniaxial compressive strengths of wet brick elements and brick–mortar components, resulting from tests on cylindrical cores with height-to-depth ratios of around two, are shown to be 13–18% lower than those in ambient-dry conditions. The tests also show that enhanced confinement levels in brick units mobilise 67–92% higher strengths than in the corresponding unconfined cylinders. Moreover, experimental observations indicate that the presence of significant confinement reduces the influence of moisture on the mechanical properties as a function of the brick and mortar joint thickness and their relative stiffness. As a result, the failure of wet masonry walls in compression is found to be only marginally lower than those in ambient-dry conditions. Based on the test results, the influence of moisture on the constitutive response and mechanical properties of masonry components is discussed, and considerations for practical application are highlighted.

Highlights

  • Clay bricks and stone blocks have been widely used as the main construction materials in historic structures

  • The tests described in this paper show that core masonry samples with mortar joints and h/d [ 2.0, (CBW and CCW) in wet conditions, having a moisture content of about 10% by weight had a lower compressive strength of about 14–18% in comparison to those in ambient-dry conditions (CBD and CBW) with a moisture content of about 2.5% by weight

  • This paper described an experimental investigation into the fundamental mechanical properties of masonry elements incorporating fired-clay bricks and hydraulic lime mortars under ambient-dry and wet conditions, corresponding to 48 h of submersion in water

Read more

Summary

Introduction

Clay bricks and stone blocks have been widely used as the main construction materials in historic structures. These are rarely provided with protection systems against moisture or rising damp, nor against significant temperature variations. Amongst the main causes of degradation of heritage masonry is the presence of high moisture content resulting from the capillary absorption of groundwater. Compressive tests on brick units submersed in water were shown in previous studies to have a lower strength in comparison to their dry counterparts [5]. Average elastic modulus-to-compressive strength ratios obtained from tests on prismatic samples were found to be 14% lower for specimens with high moisture in comparison to those in dry conditions [7]. Other tests on compression elements showed a significant drop in capacity in the range of 60% for a moisture content of 15.81% by weight compared to their counterparts for a 3.5% moisture content by weight [8]

Methods
Results
Conclusion

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.