Abstract

Two series of thermoplastic polyurethane elastomers [poly(propylene glycol) (PPG) based PP samples and poly(oxytetramethylene)glycol (PTMG) based PT samples] were synthesized from isophorone diisocyanate (IPDI)/1,4-butanediol (BD)/PPG and IPDI/BD/PTMG. The IPDI/BD based hard segments contents of polyurethane prepared in this study were 40–73 wt %. These polyurethane elastomers had a constant soft segment molecular weight (average Mn, 2000) but a variable hard segment block length (n, 3.5–17.5; average Mn, 1318–5544). Studies were made on the effects of the hard segment content on the dynamic mechanical thermal properties and elastic behaviors of polyurethane elastomers. These properties of PPG based PP and PTMG based PT samples were compared. As the hard segment contents of PP and PT samples increased, dynamic tensile modulus and α-type glass transition temperature (Tg) increased; however, the β-type Tg decreased. The permanent set (%) increased with increasing hard segment content and successive maximum elongation. The permanent set of the PT sample was lower than that of the PP sample at the same hard segment content. © 1998 John Wiley & Sons, Inc. J Appl Polym Sci 69: 1349–1355, 1998

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.