Abstract
Introduction. The main approaches to long-term creep tests of concrete regulated by GOST 24544-2020, valid in the Russian Federation, as well as foreign ISO, ASTM, and EN standards, are analyzed.Aim. In this work, fundamental differences in conducting tests following Russian and foreign standards are determined. These efforts are essential and urgent, since, in order to use test results obtained abroad in Russia, it is necessary to harmonize test methods and initial test parameters (samples, measuring and test equipment, etc.).Materials and methods. The article reviews testing procedures, controlled parameters, and processing of result; part 1 of the article covered the application, testing and measuring equipment, manufacturing process, sample parameters and fittings, and test preparation.Results. ISO, ASTM, and EN are comparable; however, they differ greatly from GOST 24544 in some respects, in particular, regarding the sample parameters and the methods of their installation in the testing equipment.Conclusion. Further harmonization of GOST 24544 with the aforementioned foreign standards is necessary.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
More From: Bulletin of Science and Research Center of Construction
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.