Abstract

Aluminum matrix composites containing of 10, 20 and 30 vol% TiB2 particles were compacted by underwater and direct shock wave consolidation methods. SEM and Optical Microscopic examination, hardness and bending strength measurements were used to characterize the samples. It is observed that there were different distributions of TiB2 particles in recovered compacts by each method. In the direct method, the distribution of TiB2 particles at the center and at the periphery of the sample was different whereas in the underwater method there was a uniform microstructure in the sample. The microhardness of the compacts increased with increasing TiB2 particle volume fraction in both methods. The results showed highest bending strength for the composite containing 20 vol% TiB2 particles.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.