Abstract

In this paper, white Portland cement was used as an experimental material. Prismatic specimens with pre-existing flaws at different angles of inclination (α) varying through 0°, 30°, 45°, 60°, 75° to 90° and cylindrical specimens with different numbers of pre-existing flaws (n) varying through 0, 1, 2 to 3 were tested under uni-axial compression tests. Crack initiation, propagation, coalescence, and failure were observed. The corresponding analytical expression for the stress intensity factor under uni-axial compression was derived, the coefficient of friction and the stress intensity factor of the specimens on the surfaces of the crack were analysed, and the corrective coefficient for the stress intensity factor was introduced. Fatigue tests with a loading frequency of f = 100 Hz were carried out on cylindrical specimens with constant amplitude of the cyclic load which is a proportion of the compressive load at failure (F f) obtained from the uni-axial compression tests. The fatigue property of the specimens was analysed and the relationship (S max − lg N f) between the maximum stress and the number of loading cycles at failure for specimens with pre-existing flaws was proposed. The effect of pre-existing flaws on the fatigue life (N f) and dynamic load (S D) which can be applied was investigated.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.