Abstract

ABSTRACT Combining poly (L-lactic acid) (PLLA) with thermoplastic polyurethane elastomer (TPU) can integrate the advantages of excellent biocompatibility and intrinsic shape memory ability of PLLA and high elasticity and excellent shape memory properties of TPU in the application of minimally invasive surgery for bone tissue engineering. However, TPU easily forms a sea-island-like structure in PLLA matrix, decreasing shape memory properties. In this study, a co-continuous structure of TPU phase in PLLA matrix was constructed by adding Fe3O4 nanoparticles due to the changed interfacial tension and flow behavior of TPU, which endowed the TPU/PLLA/Fe3O4 blend fabricated via selective laser sintering (SLS) with excellent shape memory properties. As a result, the morphology of TPU in the blend changed from sea-island-like structure to complete co-continuous structure with increasing Fe3O4 content (0 to 10wt%), and shape recovery ratios in 50 °C water increased from 66.67 to 95.92%. The introduction of Fe3O4 endowed the blend with magnetic responsive shape memory in alternating magnetic field because Fe3O4 could heat it by generating heat from relative friction and particle collisions. Besides, the tensile modulus and hardness of the specimen with 10wt% Fe3O4 nanoparticles increased. In addition, the blend demonstrated excellent biocompatibility by promoting cell adhesion, spreading, and proliferation.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.