Abstract

Chitosan scaffolds of different deacetylation degrees, average molecular weights and concentrations reinforced with silica nanoparticles were prepared for bone tissue regeneration. The resulting nanocomposites showed similar pore sizes (<300 μm) regardless the deacetylation degree and concentration used in their formulation. Their mechanical compression resistance was increased by a 30% with the addition of silica nanoparticles as nanofillers. The biocompatibility of the three-dimensional chitosan scaffolds was confirmed by the Alamar Blue assay in human primary osteoblasts as well as the formation of cell spheroids indicative of their great potential for bone regeneration. In vivo implantation of the scaffolds in a mice calvaria defect model provided substantial evidences of the suitability of these nanocomposites for bone tissue engineering showing a mature and dense collagenous tissue with small foci of mineralization, vascularized areas and the infiltration of osteoblasts and osteoclasts. Nevertheless, mature bone tissue formation was not observed after eight weeks of implantation.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.