Abstract
Polylactide (PLA) has been melt spun to produce multifilament continuous yarns. The thermal characteristics of PLA filaments have been investigated using modulated differential scanning calorimetry (MDSC). With MDSC, it is possible to separate the different thermal events and to analyze them more precisely. The influence of hot drawing on thermal properties of PLA filaments has been studied. Hot drawing promotes an increase of glass transition temperature ( T g) and a decrease of heat capacity. The cold crystallization spreads on a larger range of temperature and the peak occurs at a lower temperature. The initial degrees of cristallinity of PLA filaments have been calculated thanks to the reversing and non reversing curves of MDSC. Tensile properties of PLA filaments are also investigated.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.