Abstract
Direct laser deposition of Ni-Cr-Mo alloy has been carried out to study the phase structure transformation under various operating parameters. To assess the phase composition SEM, TEM and XRD analysis were performed. It clearly seen that the precipitation of straightening phases (γ' and γ") depends on the temperature gradients caused by different laser power. The nucleation of γ' phase starts at 750 W while γ" phase at 1000 W. The changes in temperature gradients lead to different diffusion condition across all the stage of laser power variation and formation of δ-phase, primary MC carbides and Laves phase. δ-phase of all samples did not change the shape and characterized only by plate-like shape.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.