AbstractPolycrystalline silicon (poly-Si) thin films (∼700nm) were deposited by LPCVD, doped with 950°C phosphorous diffusion, and rendered porous by anodization and stain etching. From x-ray photoelectron spectroscopy, poly-Si films have atomic concentration of C(ls):0(ls):Si(2p) = 6%:15%:79%. However, porous poly-Si (PPS) films with weak photoluminescence (PL) have C:O:Si of 20%:38%:42%. For PPS films with strong PL, C:O:Si is 11%:38%:51%. From micro-Raman, scattered spectra for 632nm laser source has peak at 735nm and full wave half maximum (FWHM) of 76nm, and is similar to the PL spectra excited by 400nm uv laser source. High resolution transmission electron microscopy (TEM) study shows that PPS film is of complex structure and composes of numerous Si nano-crystals (1∼10nm) surrounded by amorphous materials.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.